Sintered SmCo Magnets 1

Sintered SmCo Magnets

It’s a high performance, low temperature coefficient permanent magnet with its high working temperature—350 degree centigrade. When working above 180 degree centigrade, its maximum energy product BH and steady temperature are superior than NdFeB magnetic materials. It needn’t to be coated because it is difficult to be eroded and oxidized. SoCo magnet is widely used in motors, watch, transducers, instruments, positional detector, generators, radar communications, medical equipments, various magnetism spreading devices, magnetic processor, electrical engineering and magnetic derrick.

You can fin d the characteristics as follows,

Material
Code
Remanence Br
Coercivity Force
Intrinsic Coercivity
Maximum Energy
Curie
Maximum Operating
Force
Product Bhm
Temperature
Temperature
Br
bHc
iHc
(BH)max
TC
TW
T
KGs
KA/m
KOe
KA/m
KOe
KJ/m3
MGOe
°C
°C
Sintered
YX-18
0.85-0.9
8.5-9.0
620-648
7.8-8.2
1194-1513
15-19
127-143
16-18
750
250
SmCo1:5
YX-20
0.92-0.96
9.2-9.6
653-717
8.2-9.0
1194-1513
15-19
150-167
19-21
750
250
YX-24
0.96-1.0
9.6-10.2
730-770
9.2-9.7
1194-1513
15-19
175-190
22-24
750
250
YXG-24
0.95-1.02
9.5-10.2
637-732
8.0-9.2
1433-1990
18-25
175-190
22-24
800
350
smCo2:17
YXG-26
1.02-1.05
10.2-10.5
748-796
9.4-10.0
1433-1990
18-25
195-215
24-26
800
350
YXG-28
1.05-0.08
10.5-10.8
756-796
9.5-10.0
1433-1831
18-25
205-220
26-28
800
350
YXG-28B
1.02-1.10
10.2-11.0
420
5.2-5.6
440-520
5.5-6.5
205-220
26-28
800
350
YXG-30
1.08-1.10
10.8-11.0
780
9.8-10.5
955-1195
18-25
220-240
28-30
800
350
YXG-30B
1.08-1.15
10.8-11.5
420
5.2-5.6
440-520
5.5-6.5
220-240
28-30
800
350
Bonded
Yb-6
0.4
4.0
280
3.5
800
10
30-50
4-6
120
smCo1:5
Yb-10
0.5
5.0
320
4.0
800
10
50-65
6-8
120
YbG-10
0.6
6.0
360
4.5
800
10
65-80
8-10
120
smCo2:17
YbG-12
0.7
7.0
400
5.0
800
10
85-95
10-12
120